Suggestion - Using Flux in Small Vessel
jseaz73 opened this issue ยท 1 comments
When making a mistake in an alloy mixture...
Here is what I did ...
1 vessel - 500 mb of Silver
1 vessel - 500 mb of Gold
1 vessel - 1500 mb of Copper.
I mixed the gold and silver together
then added the gold and silver to the copper ...
but now I have 1500 of copper & 1000 of unknown ... just like real life, adding flux to a molten vessel will cause the slag to form and be able to get separated
I suspect what I should have done is Add the Silver and the gold to the Copper ...