This is a problem with rose gold alloy.
there is a non-heated alloy manufacturing method where copper, gold, and rose gold are made in a 1:1:1 ratio,
and a heated method where it is made in a 1:1:2 ratio.

However, even if the burner is lit, if you pour it little by little (less than 111mb) by pipe or basic tank unit into a basin, it will be created in a non-heated manner. (1:1:1 ratio)

So, you need to automate it by first lighting the fire, then pour using a bucket, (more than 111mb at a time), and then putting it in through a pipe or something.

Solution(s)

So I think, At least if the burner is lit, I hope it can be made only by heating method.

Describe alternatives you've considered

or, I just thought about changing this to this.

Non-heated method (11:11:11 mb)
Heated method (111:111:222 mb)

->

Heated method (11:11:22 mb)
Non-heated method (111:111:111 mb)